Customer Challenge:
Lack of lubrication and potential wear affecting the combustion process.
Oerlikon Solution:
- BALINIT® DLC Star coating provides reliable protection for injection parts against wear
- Supports lower friction
Choose your country / language
Customer Challenge:
Lack of lubrication and potential wear affecting the combustion process.
Oerlikon Solution:
Solución | Material de recubrimiento | Tecnología de recubrimiento | Dureza recubrimiento HIT [GPa] | Coeficiente de fricción (en seco) frente al acero | Temp. máx. de trabajo [°C] | Temperatura de proceso [°C] | |
---|---|---|---|---|---|---|---|
CrN / a-C:H | PACVD | ~15-25 | 0.1 - 0.2 | 300 | < 250 | ||
a-C:H:W / a-C:H | PVD / PACVD | ~15-25 | 0.1 - 0.2 | 300 | < 250 |
|
|
ta-C | Arc | > 40 | 0.1 - 0.2 | 450 | - |