Customer Challenge:
Lack of lubrication and potential wear affecting the combustion process.
Oerlikon Solution:
- BALINIT® DLC STAR coating provides reliable protection for injection parts against wear
- Supports lower friction
Choose your country / language
Customer Challenge:
Lack of lubrication and potential wear affecting the combustion process.
Oerlikon Solution:
Solução | Material de revestimento | Tecnologia de Revestimento | Dureza do revestimento HIT [GPa] | Coeficiente de atrito (a seco) em oposição ao aço | Temp. máx. de operação [°C] | Temperatura do processo [ºC] | |
---|---|---|---|---|---|---|---|
CrN / a-C:H | PACVD | ~15-25 | 0,1 - 0,2 | 300 | < 250 | ||
CrN | Sputter | 18 +/-3 | ~0,5 | 700 | < 250 |