Customer Challenge:
High wear and noise emission caused by stick-slip phenomena.
Oerlikon Solution:
Implement BALINIT® DLC STAR or BALINIT® C coatings for smooth operation and noise level reduction.
Choose your country / language
Customer Challenge:
High wear and noise emission caused by stick-slip phenomena.
Oerlikon Solution:
Implement BALINIT® DLC STAR or BALINIT® C coatings for smooth operation and noise level reduction.
Solution | Matériau de revêtement | Technologie de revêtement | Dureté du revêtement HIT [GPa]. | Coefficient de friction (sec) acier | Temp. de service max. [°C] | Température du procédé [°C] | |
---|---|---|---|---|---|---|---|
CrN / a-C:H | PACVD | ~15-25 | 0.1 - 0.2 | 300 | < 250 | ||
CrN + a-C:H:Me (WC/C) | Sputter | 8-12 / 12-15 | 0.1 - 0.2 | 300 | < 250 | ||
a-C:H:Me (WC/C) | Sputter | 10 - 15 | 0.1 - 0.2 | 300 | < 250 |