Customer Challenge:
High friction and wear
Oerlikon Solution:
- Minimizing friction to reduce power loss
- Enhancing performance
- Improving reliability
- Facilitating lighter design
Choose your country / language
Customer Challenge:
High friction and wear
Oerlikon Solution:
Solution | Matériau de revêtement | Technologie de revêtement | Dureté du revêtement HIT [GPa]. | Coefficient de friction (sec) acier | Temp. de service max. [°C] | Température du procédé [°C] | |
---|---|---|---|---|---|---|---|
CrN / a-C:H | PACVD | ~15-25 | 0.1 - 0.2 | 300 | < 250 | ||
a-C:H:W / a-C:H | PVD / PACVD | ~15-25 | 0.1 - 0.2 | 300 | < 250 |
|