Customer Challenge:
Soot deposition on sealing areas of the valve resulting in reduced compression and lower efficiency.

Oerlikon Solution:
Applying CrN coating to prevent adhesions on the surface/sealing area, ensuring high engine efficiency and reliability.

Solution Matériau de revêtement Technologie de revêtement Dureté du revêtement HIT [GPa]. Coefficient de friction (sec) acier Temp. de service max. [°C] Température du procédé [°C]
CrN Sputter 18 +/-3 ~0.5 700 < 250
téléchargement
CrN / a-C:H PACVD ~15-25 0.1 - 0.2 300 < 250
téléchargement