语言切换
轻松快捷地为您的应用找到正确的表面处理解决方案
解决方案 | 涂层材料 | 涂层技术 | 涂层硬度HIT [GPa] | 摩擦系数(干)与钢的比较 | 最高工作温度[°C] | 工艺温度[°C] | |
---|---|---|---|---|---|---|---|
MoN | Sputter / Arc | 15 – 35 depending on application | - | 800 | - | ||
ta-C | Arc | > 40 | 0.1 - 0.2 | 450 | - | ||
TiN | Arc | 30 +/- 3 | ~ 0.6 | 600 | < 350 | ||
AlTiN | Arc | 30 +/- 3 | ~ 0.6 | 900 | < 350 | ||
AlTiN | Arc | ≥ 20 | 0.4 - 0.5 | - | 250 - 300 | ||
TiN:Ag | Arc | 25 - 29 | ~ 0.5 | - | < 350 | ||
a-C:H:W (WC/C) | Sputter | 8-12 / 12-15 | 0.1 - 0.2 | 300 | < 250 | ||
CrN | Sputter | 18 +/- 3 | ~0.5 | 700 | < 250 | ||
a-C:H | PACVD | ~ 15 - 25 | 0.1 - 0.2 | 300 | < 250 | ||
CrN + a-C:H | PACVD | ~ 15 - 25 | 0.1 - 0.2 | 300 | < 250 | ||
TiAlN | Arc | 33 +/- 3 | ~0.6 | 700 | < 350 | ||
TiCN | S3p | ≥ 35 | ~ 0.6 | - | < 400 | ||
氮化锆 | Arc | 20 - 25 | 0.5 | 500 | 350 | ||
TiN | Arc | 30 +/- 3 | ~0.6 | 600 | < 500 |
|
|
a-C:H:Me (WC/C) | Sputter | 10 - 15 | 0.1 - 0.2 | 300 | < 250 | ||
CrN + a-C:H:Me (WC/C) | Sputter | 8-12 / 12-15 | 0.1 - 0.2 | 300 | < 250 | ||
TiN + a-C:H | PACVD | ~25-35 | 0.1 - 0.2 | 350 | 250 - 350 | ||
CrN | Sputter | 18 +/-3 | ~0.5 | 700 | < 250 | ||
CrN | Arc | 25+/-3 | ~0.5 | 700 | 500 | ||
CrN | Arc | 18+/-3 | ~0.5 | 700 | - |
|
|
a-C:H | PACVD | ~15-25 | 0.1 - 0.2 | 300 | < 250 | ||
CrN / a-C:H | PACVD | ~15-25 | 0.1 - 0.2 | 300 | < 250 | ||
a-C:H:Si | PACVD | ~ 15-25 | 0.05 - 0.2 | 350 | < 220 | ||
TiAlN | Arc | 33 +/- 3 | ~0.6 | 900 | 500 |
|
|
ta-C | Filtered Arc | 35 - 50 | 0.1 - 0.2 | 450 | < 100 | ||
TiAlN | Arc | 32 +/- 2 | ~0.6 | 700 | < 500 | ||
非晶碳 | S3p | 30 - 40 | 0.1 - 0.2 | 350 | < 200 | ||
CrN / a-C | S3p | 30 - 40 | 0.1 - 0.2 | 350 | < 200 |
|
|
- | - | - | - | - | - | ||
- | - | - | - | - | - | ||
- | - | - | - | - | - | ||
NiCrAlY (Ni, Ni/Co, Co) | Arc | 7 - 11 | - | 1200 | 400 - 500 |
|
|
- | - | - | - | - | - |
© Copyright 2024 OC Oerlikon Management AG