语言切换

Compressor Wheel / Impeller

Customer Challenge:
Particle erosion and corrosion due to water condensation.

Oerlikon Solution:
Implement BALINIT® TURBINE PRO or AlCrN-based coatings with specialized process control.

For information about our AlCrN-based BALINIT® coatings please click here.

解决方案 涂层材料 涂层技术 涂层硬度HIT [GPa] 摩擦系数(干)与钢的比较 最高工作温度[°C] 工艺温度[°C]
TiAlN Arc 32 +/- 2 ~0.6 700 < 500
下载
ta-C Filtered Arc 35 - 50 0.1 - 0.2 450 < 100
下载