Cam Shaft

Customer Challenge:
High friction and wear

Oerlikon Solution:

  • Minimizing friction to reduce power loss
  • Enhancing performance
  • Improving reliability
  • Facilitating lighter design
Soluzione Materiale di rivestimento Tecnologia Coating Durezza del rivestimento HIT [GPa] Coefficiente d’attrito (a secco) vs. acciaio Massima temp. di esercizio [°C] Temperature di processo [°C]
CrN / a-C:H PACVD ~15-25 0.1 - 0.2 300 < 250