High wear resistance and reduced friction with BALINIT® CNI, BALINIT® DLC STAR, or BALINIT® C, proven in series production.
Soluzione | Materiale di rivestimento | Tecnologia Coating | Durezza del rivestimento HIT [GPa] | Coefficiente d’attrito (a secco) vs. acciaio | Massima temp. di esercizio [°C] | Temperature di processo [°C] | |
---|---|---|---|---|---|---|---|
CrN | Sputter | 18 +/-3 | ~0.5 | 700 | < 250 | ||
CrN / a-C:H | PACVD | ~15-25 | 0.1 - 0.2 | 300 | < 250 | ||
a-C:H:W / a-C:H | PVD / PACVD | ~15-25 | 0.1 - 0.2 | 300 | < 250 |
|