Customer Challenge:
High wear and noise emission caused by stick-slip phenomena.
Oerlikon Solution:
Implement BALINIT® DLC STAR or BALINIT® C coatings for smooth operation and noise level reduction.
Choose your country / language
Customer Challenge:
High wear and noise emission caused by stick-slip phenomena.
Oerlikon Solution:
Implement BALINIT® DLC STAR or BALINIT® C coatings for smooth operation and noise level reduction.
솔루션 | 코팅 재료 | 코팅 기술 | 코팅 경도 HIT [GPa] | 마찰 계수 (건식) 대 강철 | 최대 서비스 온도 [°C] | 공정 온도 | |
---|---|---|---|---|---|---|---|
CrN / a-C:H | PACVD | ~15-25 | 0.1 - 0.2 | 300 | < 250 | ||
CrN + a-C:H:Me (WC/C) | Sputter | 8-12 / 12-15 | 0.1 - 0.2 | 300 | < 250 | ||
a-C:H:Me (WC/C) | Sputter | 10 - 15 | 0.1 - 0.2 | 300 | < 250 | ||
a-C:H:W / a-C:H | PVD / PACVD | ~15-25 | 0.1 - 0.2 | 300 | < 250 |
|