Customer Challenge:
Lack of lubrication and potential wear affecting the combustion process.
Oerlikon Solution:
- BALINIT® DLC Star coating provides reliable protection for injection parts against wear
- Supports lower friction
Choose your country / language
Customer Challenge:
Lack of lubrication and potential wear affecting the combustion process.
Oerlikon Solution:
솔루션 | 코팅 재료 | 코팅 기술 | 코팅 경도 HIT [GPa] | 마찰 계수 (건식) 대 강철 | 최대 서비스 온도 [°C] | 공정 온도 | |
---|---|---|---|---|---|---|---|
CrN / a-C:H | PACVD | ~15-25 | 0.1 - 0.2 | 300 | < 250 | ||
ta-C | Arc | > 40 | 0.1 - 0.2 | 450 | - |