Customer Challenge:
Wear and friction during dry running in start-stop cycles.
Oerlikon Solution:
Achieve high wear resistance and reduced friction with BALINIT® CNI, BALINIT® DLC STAR, or BALINIT® C, all proven effective in series production.
Choose your country / language
Customer Challenge:
Wear and friction during dry running in start-stop cycles.
Oerlikon Solution:
Achieve high wear resistance and reduced friction with BALINIT® CNI, BALINIT® DLC STAR, or BALINIT® C, all proven effective in series production.
솔루션 | 코팅 재료 | 코팅 기술 | 코팅 경도 HIT [GPa] | 마찰 계수 (건식) 대 강철 | 최대 서비스 온도 [°C] | 공정 온도 | |
---|---|---|---|---|---|---|---|
CrN | Sputter | 18 +/-3 | ~0.5 | 700 | < 250 | ||
CrN / a-C:H | PACVD | ~15-25 | 0.1 - 0.2 | 300 | < 250 | ||
a-C:H:W / a-C:H | PVD / PACVD | ~15-25 | 0.1 - 0.2 | 300 | < 250 |
|