Skiktalternativ Beläggningsmaterial Beläggningsteknik Beläggningshårdhet HIT [GPa] Friktionskoefficient (torr) vs. stål Max. driftstemp. [°C] Processtemperatur [°C]
a-C:H:Me (WC/C) Sputter 10 - 15 0.1 - 0.2 300 < 250