Dental abutments Proven biocompatibility of connecting elements

Solution Coating material Coating technology Coating hardness HIT [GPa] Coefficient of friction (dry) vs. steel Max. service temp. [°C] Process temperature [°C]
TiN Arc 30 +/- 3 ~ 0.6 600 < 350
Download
TiCN S3p ≥ 35 ~ 0.6 - < 400
Download
ZrN (Zirconium Nitride) Arc 20 - 25 0.5 500 350
Download