Solution Coating material Coating technology Coating hardness HIT [GPa] Coefficient of friction (dry) vs. steel Max. service temp. [°C] Process temperature [°C]
TiN Arc 30 +/- 3 ~ 0.6 600 < 350
Download
a-C:H PACVD ~ 15 - 25 0.1 - 0.2 300 < 250
Download
a-C:H:W (WC/C) Sputter 8-12 / 12-15 0.1 - 0.2 300 < 250
Download
TiAlN Arc 33 +/- 3 ~0.6 700 < 350
Download
TiN:Ag Arc 25 - 29 ~ 0.5 - < 350
Download
TiCN S3p ≥ 35 ~ 0.6 - < 400
Download
ZrN (Zirconium Nitride) Arc 20 - 25 0.5 500 350